Tensile Strain Hardening Exponent - ISO 10275

ISO 10275:2007 specifies a method for determining the tensile strain hardening exponent, commonly called the n-value, of flat metallic materials, typically sheet and strip.

To calculate the n-value a test is performed to ISO 6892 and using the axial extensometer a stress strain curve is produced. The n-value is calculated over the whole uniform plastic strain range. This is typically from the begining of uniform strain hardening region, after any yield point phenomena, up until just before the point at which tensile strength is calculated, Rm. These calculations can be done automatically using Bluehill (not lite) or Partner software.

An ISO 10275 test is typically performed at the same times as ISO 10113, plastic strain ratio.

このソリューションについて

関連試験規格: ASTM E517 | ASTM E646 | ISO 6892-1
試験片タイプ: N/A
Materials: 金属
試験形式: 引張
ビジネスセクター: 工業製品 | 自動車/鉄道/造船
ISO-10113 W E402
You are viewing a static image in place of an informative flash animation. Please download Adobe® Flash Player and refresh this page to view the animation.
このソリューションへのご質問などは・・・
お問合せください

関連資料

2630シリーズ伸び計   2630シリーズ伸び計
5900 シリーズ試験結果のゆるぎなき信頼性   5900 シリーズ試験結果のゆるぎなき信頼性
金属試験ソリューション カタログ   金属試験ソリューション カタログ

弊社デモルーム

インストロンジャパンのデモルームで、実際に試験機をご覧頂くことができます。また、試験片をお持ちいただき、適切なグリップなどのアクセサリーについてご相談いただくことも可能です。
詳しくはお問合せください。